欢迎访问Taizhou Huayuan Metallurgical Machinery Co., Ltd.网站!
中文 中文 |  英语 English

Roller hearth heat treatment furnace furnace roller furnace bottom roller nodule related problems

时间:2020-06-13   访问量:1588

1. The non-oxidation (nitrogen protection) roller hearth heat treatment furnace (normalized furnace) heated by radiant tube is used for a period of time. The furnace roller and furnace bottom roller are nodular. The direct hazard of nodulation is to cause pits in the thicker steel plate. And affect the surface quality, as shown in the following figure, please talk about the effective measures to prevent the furnace bottom roll nodule and the treatment after nodulation.


2. Casting has pores, trachoma and other congenital deficiencies in the density of the drawing. The drawing is made of hot-rolled bar material, and through multiple processes such as perforation and tube drawing, the uniformity and density of the ingredients are better than the casting. The price is much higher than the price. Without considering the brand, the stove and the stove are very different from the price. All said the same material. The service life is much better.


3. In the general protective atmosphere, roller hearth furnace will have nodule phenomenon on the roller hearth roller surface, which is difficult to solve. I ask SAC President Mr. Han Hengji and Mr. LOI Su, they think that the thick plate is on the roller bottom Nodules in the furnace are mainly caused by surface impurities such as oxide scales in contact with the roller table at high temperatures, and once nodules will scratch the workpiece and exacerbate nodules. The only solution is to add a shot blasting unit in front of the furnace, to remove oxide scales, and to wash away impurities such as steel shots. Even if the shot blasting unit is added, there is no guarantee that no lumps will be formed at all. Regular inspections are required!


4. However, foreign experts say that the outer surface of the roller using centrifugal casting is not processed better, it can maintain a dense structure, but the adsorption force of iron oxide scale or other impurities is weak at high temperature, but the inner surface has been machined with an accuracy of 12.5 , Can effectively ensure the uniformity of the wall thickness of the roller.

912492605.jpg

上一篇:Knowledge of coating operation process in centrifugal castings

下一篇:没有了!

相关新闻

为您提供耐腐耐磨砂浆泵,工程塑料泵,蒸发循环泵等方面的专属解决方案

联系我们

联系人:Manager Zhang

手机:(86)15195227247

电话:(86)0523-88551112

邮箱:464292064@qq.com

地址:Industrial concentration area (Weijia Village), Zhangdian Town, Jiangyan District, Taizhou City

Copyright © 2020-2021 Taizhou Huayuan Metallurgical Machinery Co., Ltd. All Rights Reserved 备案号码:苏ICP备20031998-1号

服务咨询热线

(86)15195227247

提供完善的冶金机械解决方案

微信扫一扫

微信联系
返回顶部